News: Microelectronics
26 November 2026
1.5kV GaN monolithic bidirectional switch on 8-inch silicon
Researchers based mainly in China report the demonstration of an enhancement-mode high-voltage monolithic bidirectional switch (MBDS) developed on an 8-inch gallium nitride (GaN)-on-silicon (Si) platform using a method compatible with mainstream silicon electronics [Yingfei Sun et al, IEEE Transactions on Electron Devices, online 26 October 2026]. The team claims the first demonstration of a GaN BDS with a static breakdown voltage (BV) of more than 1.5kV on an 8-inch silicon substrate.
The MBDS process flow was gold-free with a view to enabling integration with low-cost mainstream silicon complementary metal–oxide–semiconductor (CMOS) transistor circuitry. Gold is widely used in GaN transistor manufacturing, but is poisonous to silicon CMOS performance. Enhancement (E)-mode devices (i.e. normally-off at 0V gate potential) are particularly favored in power applications due to reduced power consumption and to providing a safer situation in conditions of failure.
The team from University of Science and Technology of China, Suzhou Institute of Nano-Tech and Nano-Bionics and Xi’an Jiaotong–Liverpool University in China, University of Liverpool in the UK, and Guangdong Institute of Semiconductor Micro-Nano Manufacturing Technology in China, see their results as demonstrating “wafer-level manufacturability, bidirectional high-voltage potential, and basic switching functionality of the proposed 8-in GaN-on-Si MBDS platform.”
The researchers see potential for their MBDS deployment in high-efficiency power conversion as components of matrix converters, solid-state circuit breakers, T-type converters, bidirectional DC–DC converters, and battery management systems. By integrating the BDS in a monolithic format the device reduces the chip area and hence on-resistance power losses.
The epitaxial material for the MBDS (Figure 1) was grown by metal-organic chemical vapor deposition on 8-inch silicon: 5.1μm GaN buffer, 500nm GaN channel, 0.5nm aluminium nitride (AlN) spacer, 15nm Al0.15Ga0.85N barrier, and 80nm p-GaN gate.

Figure 1: p-GaN gate HEMT and the p-GaN gate MBDS on 8-inch CMOS-compatible architecture.
The gate was defined first in the transistor fabrication (Figure 2) to give a self-aligned structure. The gate process consisted of 100nm titanium nitride (TiN) deposited on the p-GaN and then patterned and etched. The TiN etch was achieved first with inductively-coupled plasma, and then a wet process to give a lateral undercut. The p-GaN was then plasma etched using a highly selective process recipe. The surface roughness after etching was 0.6nm, according to atomic force microscope (AFM) analysis.

Figure 2: Fabrication process flow, highlighting self-aligned gate-first process and AFM image of result.
The first interlayer dielectric (ILD1) passivation consisted of atomic layer deposition (ALD) AlN and 150nm plasma-enhanced CVD (PECVD) silicon dioxide (SiO2).
The team explains: “The ALD-AlN layer is used to mitigate surface-state-related trapping and leakage, whereas the PECVD-SiO2 layer provides the dielectric thickness required for subsequent field-plate integration.”
Separate devices were isolated from each other by nitrogen ion implants. Annealed ohmic metals were used for the transistor source and drain electrodes: Ti/Al/Ti/TiN.
A further 100nm PECVD SiO2 was used for ILD2, and 130nm for ILD3. Source (S)-connected field plates (FPs) were implemented: the lower FP1 consisting of TiN/Al/TiN, while the upper FP2 was TiN.
In the dual-gate MBDS the field plates were placed symmetrically: “This arrangement is referred to as the symmetric D-SFP configuration and is designed to provide staged electric-field modulation under both blocking polarities.”
The aim was to avoid the field peaking above critical and so not prematurely breaking down in the off-state.
Two metal (M1, M2) interconnection layers were enabled with intermetal dielectrics (IMDs), along with tungsten-plug (W-plug) and via processing.
The HEMT featured a 2μm gate (LG) separated from the source (LSG) and drain (LGD) by 2μm and 18μm, respectively. The threshold was 0.86V, giving normally-off/enhancement-mode operation. The on-resistance (RON) was 14.8Ω-mm. The gate leakage current was 30nA/mm at 6V. The off-state breakdown voltage (BV) was 1.5kV for 1μA/mm leakage. A device without FPs only managed 850V BV.
The ratio of dynamic/static RON was less than 1.3 for stressing up to 800V. The researchers say that this “is significantly better than reported values for conventional p-GaN gate HEMTs. This behavior is consistent with the combined electric-field management of the D-SFP configuration and the surface stabilization provided by the stacked passivation scheme, which reduce the peak electric field at the gate edge and suppress surface trapping, respectively, thereby mitigating electron injection under high-drain-bias OFF-state stress.”

Figure 3: (a) Equivalent circuit diagram and four-quadrant operation modes, p-GaN MBDS: (b) transfer characteristics with VG2S2 at 0V, (c) transfer characteristics with VG2S2 at 5V, (d) bidirectional output characteristics with VG2S2 at 0V, and (e) bidirectional output characteristics with VG2S2 at 5V.
The threshold for the MBDS was around 0.83V (Figure 3). The RON was near symmetric: 14.7Ω-mm and 14.9Ω-mm in the opposite flow directions. The device length was 25μm, including 3μm for the contact transfer length, so LS1S2 is 22μm. The calculated specific on-resistances (RON,SP) were 3.68mΩ-cm2 and 3.72mΩ-cm2.
The researchers also compare their work with that of other groups (Figure 4). The team comments: “The results indicate that the static BV of the present device is among the highest reported for GaN bidirectional switches fabricated on silicon substrates.”

Figure 4: (a) OFF-state bidirectional blocking characteristics and (b) benchmark of RON,SP versus static BV comparing GaN MBDSs on different substrates. Orange dashed line: theoretical limit for GaN monolithic bidirectional switches.
The group attributes the high static blocking performance to “the combined electric-field management of the D-SFP configuration and the surface stabilization provided by the ALD-AlN/PECVD-SiO2 passivation.”
The BV and RON,SP values result in a 0.61GW/cm2 Baliga figure of merit (BFOM, BV2/RON,SP). The researchers also tested the circuit under temperatures up to 150°C and 60Hz alternating current (AC) chopping behavior with up to 5kHz drive signal.
GaN monolithic bidirectional switch GaN 8-inch silicon ALD PECVD
https://doi.org/10.1109/TED.2026.3743817
The author Mike Cooke is a freelance technology journalist who has worked in the semiconductor and advanced technology sectors since 1997.